产品描述

NORYL PPO EXNL0304物性表

10% glass filled non-halogenated FR mPPE-HIPS

TYPICAL PROPERTIES (1)
MECHANICAL机械性能
Value Unit Standard
Tensile Stress, yld, Type I, 5 mm/min / 抗张程度,屈服,类型I,5 mm/min
86
MPa
ASTM D 638
Tensile Stress, brk, Type I, 5 mm/min / 抗张程度,断裂,类型I,5 mm/min
86
MPa
ASTM D 638
Tensile Strain, yld, Type I, 5 mm/min / 拉伸伸长,屈服,类型I,5 mm/min
3.3
%
ASTM D 638
Tensile Strain, brk, Type I, 5 mm/min / 拉伸伸长,断裂,类型I,5 mm/min
3.6
%
ASTM D 638
Tensile Modulus, 5 mm/min / 拉伸模量,5 mm/min
4200
MPa
ASTM D 638
Flexural Stress, yld, 1.3 mm/min, 50 mm span / 挠曲强度, 屈服, 1.3 mm/min, 50 mm 跨距
142
MPa
ASTM D 790
Flexural Modulus, 1.3 mm/min, 50 mm span / 挠曲模量, 1.3 mm/min, 50 mm 跨距
3860
MPa
ASTM D 790
Tensile Stress, yield 5 mm/min / 抗张程度,屈服, 5 mm/min
90
MPa
ISO 527
Tensile Stress, break, 5 mm/min / 抗张程度,断裂,5mm/min
89
MPa
ISO 527
Tensile Strain, yield, 5 mm/min / 拉伸伸长,屈服,5mm/min
3
%
ISO 527
Tensile Strain, break, 5 mm/min / 拉伸伸长,断裂,5mm/min
3.2
%
ISO 527
Tensile Modulus, 1 mm/min / 拉伸模量,1 mm/min
4900
MPa
ISO 527
Flexural Stress, yield, 2 mm/min / 弯曲强度,屈服,2 mm/min
152
MPa
ISO 178
Flexural Modulus, 2 mm/min / 弯曲模量,2 mm/min
4400
MPa
ISO 178
IMPACT
Value Unit Standard
Izod Impact, unnotched, 23°C / 无缺口悬臂梁冲击 23°C
502
J/m
ASTM D 4812
Izod Impact, unnotched, -30°C
484
J/m
ASTM D 4812
Izod Impact, notched, 23°C / 悬臂梁缺口冲击强度23°C
78
J/m
ASTM D 256
Izod IMPACT, notched, -30°C / 悬壁梁缺口冲击强度, -30°C
66
J/m
ASTM D 256
Izod IMPACT, notched 80*10*4 +23°C / 悬壁梁缺口冲击强度,80*10*4 +23°C
7
kJ/m2
ISO 180/1A
THERMAL
Value Unit Standard
HDT, 1.82 MPa, 3.2mm, unannealed / 热变形温度,1.82 MPa, 3.2mm,未退火
138
°C
ASTM D 648
CTE, 23°C to 80°C, flow
6.E-05
1/°C
ISO 11359-2
CTE, 23°C to 80°C, xflow
8.E-05
1/°C
ISO 11359-2
Vicat Softening Temp, Rate B/120 / 维卡软化温度,B级/120
149
°C
ISO 306
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm / 热变形温度,1.8 MPa, 未退火,80*10*4, 64.0 mm 跨距
137
°C
ISO 75/Af
PHYSICAL
Value Unit Standard
Specific Gravity/比重
1.17
ASTM D 792
Melt Flow Rate / 熔流率, 280°C/5.0 kgf
9.1
g/10 min
ASTM D 1238
Density/密度
1.16
g/cm3
ISO 1183
Melt Volume Rate, MVR at 300°C/5.0 kg
19
cm3/10 min
ISO 1133
FLAME CHARACTERISTICS
Value Unit Standard
UL Compliant, 94V-1 Flame Class Rating (3)(4)
1.5
mm
UL 94 by GE
Source GMD, last updated:10/03/2007
Processing
Parameter
Injection Molding
Value Unit
Drying Temperature / 干燥温度
100 – 120
°C
Drying Time / 干燥时间
2 – 3
hrs
Melt Temperature / 熔体温度
280 – 300
°C
Nozzle Temperature / 注嘴温度
260 – 280
°C
Front – Zone 3 Temperature / 前区3温度
280 – 300
°C
Middle – Zone 2 Temperature / 中区2温度
260 – 280
°C
Rear – Zone 1 Temperature / 后区1温度
240 – 260
°C
Hopper Temperature / 料筒温度
60 – 80
°C
Mold Temperature / 模具温度
80 – 120
°C
Source GMD, last updated:10/03/2007